Aluminum Alloys, General
Subcategory: Aluminum Alloy; Metal; Nonferrous Metal
Key Words: Aluminium Alloys, General; Al Alloys
| Component | Wt. % |  | | | Al | 87 - 100 | |
|
Material Notes: These properties are typical of commercial aluminum alloys. Some properties, such as strength and hardness, vary too much for a reasonable generalization. See entries for individual alloys for more specific information. Aluminum 1199 is the highest purity (99.99% Al min.) in the database.
Click here to view available vendors for this material.
| Physical Properties | Metric | English | Comments |
|
| Density | 2.7 g/cc | 0.0975 lb/in³ | |
Mechanical Properties |
|
| Modulus of Elasticity | 70 GPa | 10200 ksi | |
| Poisson's Ratio | 0.33 | 0.33 | |
| Shear Modulus | 26 GPa | 3770 ksi | |
Electrical Properties |
|
| Electrical Resistivity | 5e-006 ohm-cm | 5e-006 ohm-cm | |
Thermal Properties |
|
| Heat of Fusion | 390 J/g | 168 BTU/lb | |
| CTE, linear 20°C | 24 µm/m-°C | 13.3 µin/in-°F | from 0-100°C (32-212°F) |
| CTE, linear 250°C | 25 µm/m-°C | 13.9 µin/in-°F | |
| Specific Heat Capacity | 0.88 J/g-°C | 0.21 BTU/lb-°F | |
| Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
| Melting Point | 620 - 650 °C | 1150 - 1200 °F | |
| Solidus | 620 °C | 1150 °F | |
| Liquidus | 650 °C | 1200 °F | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|