Aluminum 1199-O
Subcategory: 1000 Series Aluminum; Aluminum Alloy; Metal; Nonferrous Metal
Close Analogs: Composition Notes: The aluminum content for unalloyed aluminum made by a refining process is the difference between 100.00 percent and the sum of all other metallic elements present in amounts of 0.0010 percent of more each, expressed to the third decimal before determining the sum, which is rounded to the second decimal before subtracting. When an element's specified maximum limit is 0.0XX, an observed value or a calculated value greater than 0.0005 but less than 0.0010% is rounded off and shown as " less than 0.001 ". Composition information provided by the Aluminum Association and is not for design.
Key Words: Aluminium 1199-O; Refined Aluminum; Refined Aluminium; Raffinal; Super-purity Aluminum; UNS A91199, AA11990-O
| Component | Wt. % |  | | | Al | Min 99.99 | | | Cu | Max 0.006 | | | Fe | Max 0.006 | | | Ga | Max 0.005 | |
| | Component | Wt. % |  | | | Mg | Max 0.006 | | | Mn | Max 0.002 | | | Other, each | Max 0.002 | | | Si | Max 0.006 | |
| | Component | Wt. % |  | | | Ti | Max 0.002 | | | V | Max 0.005 | | | Zn | Max 0.006 | |
|
Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.
Click here to view available vendors for this material.
| Physical Properties | Original Value | Comments |
|
| Density | 2.7 g/cc | AA; Typical |
Mechanical Properties |
|
| Hardness, Brinell | 12 | 500 kg load with 10 mm ball. Calculated value. |
| Tensile Strength, Ultimate | 45 MPa | |
| Tensile Strength, Yield | 10 MPa | |
| Elongation at Break | 50 % | In 5 cm; Sample 1.6 mm thick |
| Modulus of Elasticity | 62 GPa | In Tension; Compressive Modulus is about 2% higher |
| Poisson's Ratio | 0.33 | |
| Shear Modulus | 25 GPa | |
| Shear Strength | 34 MPa | Calculated value. |
Electrical Properties |
|
| Electrical Resistivity | 2.7e-006 ohm-cm | |
Thermal Properties |
|
| Heat of Fusion | 390 J/g | |
| CTE, linear 20°C | 23.6 µm/m-°C | 20-100ºC |
| CTE, linear 250°C | 25.5 µm/m-°C | Average over the range 20-300ºC |
| Specific Heat Capacity | 0.9 J/g-°C | |
| Thermal Conductivity | 243 W/m-K | |
| Melting Point | 660 - 660 °C | |
| Solidus | 660 °C | |
| Liquidus | 660 °C | |
Optical Properties |
|
| Reflection Coefficient, Visible (0-1) | 0.87 | |
|