Titanium Grade 12, Annealed
Subcategory: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium
Close Analogs: Titanium Grades 1,2,3,4,7,11,and 12 are all considered unalloyed and have similar mechanical properties.
Key Words: UNS R53400; ASTM Grade 12, titanium alloy
| Component | Wt. % |  | | | Mo | 0.3 | | | Ni | 0.8 | | | Ti | 98.9 | |
|
Material Notes: Addition of 0.3% Mo and 0.8% Ni to titanium increases corrosion resistance at a lower cost than Pd (see Ti Grades 7 and 11). Sample was annealed 20 min. at 815°C and 5 min. at 788°C.
Click here to view available vendors for this material.
| Physical Properties | Metric | English | Comments |
|
| Density | 4.5 g/cc | 0.163 lb/in³ | |
Mechanical Properties |
|
| Tensile Strength, Ultimate | 620 MPa | 89900 psi | |
| Tensile Strength, Yield | 480 MPa | 69600 psi | |
| Elongation at Break | 23 % | 23 % | |
| Modulus of Elasticity | 103 GPa | 14900 ksi | in tension. |
| Notched Tensile Strength | 620 MPa | 89900 psi | Kt (stress concentration factor) = 5.3 |
| Poisson's Ratio | 0.28 | 0.28 | |
| Fatigue Strength | 140 MPa | 20300 psi | at 1E+7 cycles. Kt (stress concentration factor) = 3.5 |
| Fatigue Strength | 310 MPa | 45000 psi | 1E+7 cycles, Unnotched |
| Shear Modulus | 41 GPa | 5950 ksi | |
Electrical Properties |
|
| Electrical Resistivity | 5.2e-005 ohm-cm | 5.2e-005 ohm-cm | |
Thermal Properties |
|
| Heat of Fusion | 325 J/g | 140 BTU/lb | High Purity Ti. |
| CTE, linear 20°C | 9.9 µm/m-°C | 5.5 µin/in-°F | 20-93°C |
| CTE, linear 250°C | 9.5 µm/m-°C | 5.28 µin/in-°F | Unspecified heat treatment. Average over the range 0-315ºC |
| Specific Heat Capacity | 0.555 J/g-°C | 0.133 BTU/lb-°F | |
| Thermal Conductivity | 19 W/m-K | 132 BTU-in/hr-ft²-°F | |
| Melting Point | Max 1660 °C | Max 3020 °F | Liquidus |
| Liquidus | 1660 °C | 3020 °F | |
| Beta Transus | 890 °C | 1630 °F | |
Optical Properties |
|
| Emissivity (0-1) | 0.3 | 0.3 | High purity Ti at 710°C |
| Reflection Coefficient, Visible (0-1) | 0.56 | 0.56 | High purity Ti; visible light. |
|
Printer friendly version |
References for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|