Solvay Advanced Polymers Radel® A AG-230 Polyethersulfone

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyethersulfone; Polymer; Thermoplastic

Close Analogs: This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.

Key Words: PES

Material Notes:

Data provided by the manufacturer, Amoco Corporation.

For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.

Physical PropertiesOriginal ValueComments
Density1.58 g/cc ASTM D792
Water Absorption0.42 % in 24 hours per ASTM D570

Mechanical Properties
Tensile Strength, Yield126 MPa ASTM D638
Elongation at Break1.9 % ASTM D638
Elongation at Yield1.9 % ASTM D638
Tensile Modulus8.62 GPa ASTM D638
Flexural Modulus8.07 GPa ASTM D790
Flexural Yield Strength179 MPa ASTM D790
Izod Impact, Notched0.7 J/cm ASTM D256
Tensile Impact Strength70 kJ/m² 

Electrical Properties
Electrical Resistivity1e+016 ohm-cm ASTM D257
Dielectric Constant4.1 at 1 kHz; ASTM D150
Dielectric Constant, Low Frequency4.1 at 1 kHz; ASTM D150
Dielectric Strength18 kV/mm Thickness 0.32 mm (13 mils); ASTM D149
Dissipation Factor0.002 at 1 kHz; ASTM D150
Dissipation Factor, Low Frequency0.002 at 1 kHz; ASTM D150

Thermal Properties
CTE, linear 20°C31 µm/m-°C in flow direction. ASTM E381
CTE, linear 20°C Transverse to Flow31 µm/m-°C ASTM E381
Deflection Temperature at 1.8 MPa (264 psi)213 °C ASTM D648
UL RTI, Electrical190 °C 1.57 mm
UL RTI, Mechanical with Impact190 °C 1.57 mm
UL RTI, Mechanical without Impact190 °C 1.57 mm
Flammability, UL94V-0 0.8 mm
Flammability, UL94V-0 0.8 mm
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。