Solvay Advanced Polymers Radel® A AG-330 Polyethersulfone
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.
Key Words: PES
Material Notes:
Data provided by the manufacturer, Amoco Corporation. For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.58 g/cc | ASTM D792 |
Water Absorption | 0.39 % | in 24 hours per ASTM D570 |
Mechanical Properties |
|
Tensile Strength, Yield | 126 MPa | ASTM D638 |
Elongation at Break | 1.9 % | ASTM D638 |
Elongation at Yield | 1.9 % | ASTM D638 |
Tensile Modulus | 8.62 GPa | ASTM D638 |
Flexural Modulus | 8.07 GPa | ASTM D790 |
Flexural Yield Strength | 179 MPa | ASTM D790 |
Izod Impact, Notched | 0.7 J/cm | ASTM D256 |
Tensile Impact Strength | 70 kJ/m² | |
Electrical Properties |
|
Electrical Resistivity | 1e+016 ohm-cm | ASTM D257 |
Dielectric Constant | 4.1 | at 1 kHz; ASTM D150 |
Dielectric Constant, Low Frequency | 4.1 | at 1 kHz; ASTM D150 |
Dielectric Strength | 18 kV/mm | Thickness 0.32 mm (13 mils); ASTM D149 |
Dissipation Factor | 0.002 | at 1 kHz; ASTM D150 |
Dissipation Factor, Low Frequency | 0.002 | at 1 kHz; ASTM D150 |
Thermal Properties |
|
CTE, linear 20°C | 31 µm/m-°C | in flow direction. ASTM E381 |
CTE, linear 20°C Transverse to Flow | 31 µm/m-°C | ASTM E381 |
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | ASTM D648 |
UL RTI, Electrical | 190 °C | 1.57 mm |
UL RTI, Mechanical with Impact | 190 °C | 1.57 mm |
UL RTI, Mechanical without Impact | 190 °C | 1.57 mm |
Flammability, UL94 | V-0 | 0.8 mm |
Flammability, UL94 | V-0 | 0.8 mm |
|