COMSOL CD

Advanced Elastomer Systems Santoprene® 121-62 M100 Thermoplastic Rubber

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Elastomer, TPE; Polymer; Thermoplastic

Material Notes:
A black thermoplastic high-flow elastomer for excellent injection molding performance with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and high quality SEBS compounds. It is polyolefin-based and UV stable.

Key Features: Fast, easy injection molding, especially for complex part geometries; Good sealing performance; Excellent surface aspect; Excellent elastic recovery up to 100°C (212°F); Minimal part warpage; Can be injected at lower molding temperatures or at lower injection pressures

Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC.

Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesOriginal ValueComments
Density0.91 g/cc TPE-0105 (ASTM D792)

Mechanical Properties
Hardness, Shore A62 5 Second; TPE-0169 (ASTM D 2240)
Tensile Strength, Ultimate5 MPa TPE-0153 (ASTM D 412)
Elongation at Break340 % TPE-0153 (ASTM D 412)
100% Modulus0.0021 GPa TPE-0153 (ASTM D 412)
Compression Set28 % 23°C, 168 hrs.; TPE-0016 (ASTM D 412)
Compression Set, Elevated Temperature35 % 70°C for 168 hrs.; TPE-0016 (ASTM D 412)
Compression Set, Elevated Temperature43 % 100°C, 168 hrs.; TPE-0016 (ASTM D 412)
Tensile Set10 % 23°C, 168 hrs.; TPE-0053 (ASTM D 412)

Thermal Properties
Brittleness TemperatureMax -60 °C TPE-0089 (ASTM D 746)

Processing Properties
Processing Temperature177 - 232 °C 
Drying Temperature82 °C Desiccant drying for 3 hours recommended
Dry Time3 hour 
Printer friendly version Printer friendly version


New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。