COMSOL CD

Advanced Elastomer Systems Santoprene® 121-79 W233 Thermoplastic Rubber

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Elastomer, TPE; Polymer; Thermoplastic

Material Notes:
A black thermoplastic elastomer with excellent adhesion to vulcanized thermoset EPDM rubber, specifically formulated for injection 'corner molding' applications.

Key Features: Excellent adhesion to vulcanized EPDM rubber; Specially formulated as corner molding material in automotive glass run channel to replace thermoset EPDM rubber corner molding materials; Good melt flow properties; Good compression properties; Short processing time compared to thermoset EPDM rubber

Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC.

Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.

Physical PropertiesOriginal ValueComments
Density0.93 g/cc TPE-0105 (ASTM D792)

Mechanical Properties
Hardness, Shore A79 5 Second; TPE-0169 (ASTM D 2240)
Tensile Strength, Ultimate7.4 MPa TPE-0153 (ASTM D 412)
Elongation at Break510 % TPE-0153 (ASTM D 412)
100% Modulus0.0036 GPa TPE-0153 (ASTM D 412)
Graves Tear Strength30 kN/m TPE-0056 (ASTM D 624)
Compression Set23 % 23°C, 22 hrs.; TPE-0016 (ASTM D 412)
Compression Set, Elevated Temperature52 % 70°C, 22 hrs.; TPE-0016 (ASTM D 412)
Compression Set, Elevated Temperature59 % 100°C, 22 hrs.; TPE-0016 (ASTM D 412)

Thermal Properties
Brittleness TemperatureMax -60 °C TPE-0089 (ASTM D 746)

Processing Properties
Processing Temperature177 - 232 °C 
Drying Temperature82 °C Desiccant drying for 3 hours recommended
Dry Time3 hour 
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。