Advanced Elastomer Systems Santoprene® 181-73 Thermoplastic Rubber
Subcategory: Elastomer, TPE; Polymer; Thermoplastic
Close Analogs: This grade is no longer a commercial product
Material Notes: A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, blow molding or other melt processing techniques. Drug Master File has been established at US FDA National Center for drugs and biologics. Key Features: MEM elution cytotoxicity to L-929 mouse fibroblast cells, 72 hr. exposure to rubber extract; NAmSA, MT023-100 test method; test unit, % cell lysis; typical value 0; USP physiochemical test for elastomer closures, heavy metals such as lead; NAmSA, CP020-004 test method; Test unit, ppm; typical value <1 Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding, extrusion, or blow molding. For extrusion, a general purpose screw with a compression ratio of 2.5 to 3.0 is recommended. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC. Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 0.98 g/cc | TPE-0105 (ASTM D792) |
Mechanical Properties |
|
Hardness, Shore A | 73 | 5 Second; TPE-0169 (ASTM D 2240) |
Tensile Strength, Ultimate | 8.5 MPa | TPE-0153 (ASTM D 412) |
Elongation at Break | 460 % | TPE-0153 (ASTM D 412) |
100% Modulus | 0.0036 GPa | TPE-0153 (ASTM D 412) |
Tear Strength | 28 kN/m | 28 kN/m at 23°C. Value at 100°C is 13 kN/m. TPE-0056 (ASTM D 624) |
Compression Set | 24 % | 23°C, 168 hrs.; TPE-0016 (ASTM D 412) |
Compression Set, Elevated Temperature | 38 % | 100°C, 168 hrs.; TPE-0016 (ASTM D 412) |
Tensile Set | 14 % | 23°C, 168 hrs.; TPE-0053 (ASTM D 412) |
Thermal Properties |
|
Brittleness Temperature | Max -60 °C | TPE-0089 (ASTM D 746) |
Processing Properties |
|
Processing Temperature | 177 - 232 °C | |
Drying Temperature | 82 °C | Desiccant drying for 3 hours recommended |
Dry Time | 3 hour | |
|