Advanced Elastomer Systems Santoprene® 191-70PA Thermoplastic Rubber

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Elastomer, TPE; Polymer; Thermoplastic

Material Notes:
A black thermoplastic elastomer especially formulated to be used in combination with polyamide (PA) for applications where hard/soft combinations are required. Since the product bonds to PA, typical applications are corrugated hose and fittings, soft grip handles and wheels with PA hubs. It can be processed using injection molding or extrusion.

Key Features: Excellent processing in injection molding; Smooth surface or 'soft touch'; Good rubbery properties; Excellent adhesion onto PA

Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding or extrusion. For extrusion, a general purpose screw with a compression ratio of 2.5 to 3.0 is recommended. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC.

Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesOriginal ValueComments
Density0.95 g/cc TPE-0105 (ASTM D792)

Mechanical Properties
Hardness, Shore A70 5 Second; TPE-0169 (ASTM D 2240)
Tensile Strength, Ultimate3.7 MPa TPE-0153 (ASTM D 412)
Elongation at Break270 % TPE-0153 (ASTM D 412)
100% Modulus0.0023 GPa TPE-0153 (ASTM D 412)
Graves Tear Strength22 kN/m TPE-0056 (ASTM D 624)
Compression Set28 % 23°C, 22 hrs.; TPE-0016 (ASTM D 412)
Compression Set, Elevated Temperature41 % 70°C, 22 hrs.; TPE-0016 (ASTM D 412)
Compression Set, Elevated Temperature46 % 100°C, 22 hrs.; TPE-0016 (ASTM D 412)

Processing Properties
Processing Temperature260 - 280 °C Recommended
Mold TemperatureMin 60 °C 2K molding
Mold TemperatureMin 90 °C insert molding
Drying Temperature82 °C Desiccant drying for 3 hours recommended
Dry Time3 hour 
Printer friendly version Printer friendly version


New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。