Advanced Elastomer Systems Santoprene® 241-45 Thermoplastic Rubber
Subcategory: Elastomer, TPE; Polymer; Thermoplastic
Material Notes: A colorable thermoplastic specialty elastomer which complies with NSF regulations for use in food processing equipment and plumbing applications in contact with potable water. It can be processed using injection molding, extrusion, blow molding or other melt processing techniques. Key Features: Complies with NSF Standard 61: Piping System Components for Drinking Water; Continuous temperature rating 1000 hrs. @ 135°C (275°F); Excellent flex fatigue resistance; Excellent sealing properties Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding, extrusion, or blow molding. For extrusion, a general purpose screw with a compression ratio of 2.5 to 3.0 is recommended. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC. Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 0.97 g/cc | TPE-0105 (ASTM D792) |
Mechanical Properties |
|
Hardness, Shore A | 45 | 5 Second; TPE-0169 (ASTM D 2240) |
Tensile Strength, Ultimate | 2.7 MPa | TPE-0153 (ASTM D 412) |
Elongation at Break | 270 % | TPE-0153 (ASTM D 412) |
100% Modulus | 0.0012 GPa | TPE-0153 (ASTM D 412) |
Tear Strength | 13.7 kN/m | at 23°C. Value at 100°C is 4.9 kN/m. TPE-0056 (ASTM D 624) |
Compression Set | 13 % | 23°C, 22 hrs.; TPE-0016 (ASTM D 412) |
Compression Set, Elevated Temperature | 22 % | 100°C, 22 hrs.; TPE-0016 (ASTM D 412) |
Tensile Set | 5 % | 23°C, 22 hrs.; per TPE-0053 (ASTM D 412) |
Thermal Properties |
|
Maximum Service Temperature, Air | 135 °C | Continuous temperature Rating, 1000 hours |
Brittleness Temperature | Max -60 °C | TPE-0089 (ASTM D 746) |
Processing Properties |
|
Processing Temperature | 177 - 232 °C | |
Drying Temperature | 82 °C | Desiccant drying for 3 hours recommended |
Dry Time | 3 hour | |
|