BASF Petra 110 BK-112 PET, 15% Glass Filled
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Polymer; Thermoplastic
Material Notes: Information provided by BASF Corporation.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.44 g/cc | ISO 1183 |
| Linear Mold Shrinkage | 0.005 cm/cm | MD; ASTM Test |
Mechanical Properties |
|
| Tensile Strength, Ultimate | 105 MPa | 5 mm/min; ISO 527 |
| Tensile Strength at Break | 105 MPa | 0.2 in/min; ASTM D638 |
| Elongation at Break | 3.5 % | 5 mm/min; ISO 527 |
| Elongation at Break | 3.5 % | 0.2 in/min; ASTM D638 |
| Tensile Modulus | 6.68 GPa | 1 mm/min; ISO 527 |
| Flexural Modulus | 5.35 GPa | ASTM D790 |
| Flexural Modulus | 5.48 GPa | ISO 178 |
| Flexural Strength | 145 MPa | ASTM D790 |
| Izod Impact, Notched (ISO) | 6 kJ/m² | ISO 180 |
| Charpy Impact, Notched | 0.6 J/cm² | ISO 179 |
| Izod Impact, Notched | 0.65 J/m | ASTM D256 |
Electrical Properties |
|
| Dielectric Constant | 3.3 | 1 MHz; IEC 60250 |
| Dielectric Constant | 3.4 | 100 Hz; IEC 60250 |
| Dielectric Strength | 36 kV/mm | IEC 60243-1 |
| Dissipation Factor | 0.01 | 100 Hz; IEC 60250 |
| Dissipation Factor | 0.02 | 1 MHz; IEC 60250 |
Thermal Properties |
|
| CTE, linear 20°C | 32 µm/m-°C | Parallel; ISO 11359 |
| CTE, linear 20°C Transverse to Flow | 79 µm/m-°C | ISO 11359 |
| Melting Point | 245 °C | 10 K/min |
| Melting Point | 245 °C | ASTM D3418 |
| Deflection Temperature at 0.46 MPa (66 psi) | 231 °C | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 192 °C | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 208 °C | ASTM D648 |
| Flammability, UL94 | HB | 0.81 mm |
| Flammability, UL94 | HB | 3 mm |
Processing Properties |
|
| Melt Temperature | 275 °C | Injection molding |
| Mold Temperature | 115 °C | Injection molding |
Descriptive Properties | |
| Additive | Fillers | |
| Color | BK-112 | |
| Commercial Status (March 2007) | Active America | |
| Form | Pellets | |
| Impact Modified | No | |
| Injection molding | Processable | |
| Primary Processing Technique | Injection Molding | |
| UL.UL-C | Yes | |
|