MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

BASF Ultraform N 2200 G53 UNC Q600 Acetal, 25% Glass Filled

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Acetal; Polymer; Thermoplastic

Material Notes:
Information provided by BASF Corporation.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesOriginal ValueComments
Density1.58 g/cc ISO 1183
Water Absorption0.9 % ISO 62
Moisture Absorption at Equilibrium0.15 % 23°C/50% R.H.; ISO 62
Linear Mold Shrinkage0.0072 cm/cm ISO Data; Parallel to Flow
Linear Mold Shrinkage0.014 cm/cm MD; ASTM Test
Linear Mold Shrinkage, Transverse0.0139 cm/cm ISO Data
Melt Flow4 g/10 min 190°C/2.16 kg; ISO 1133

Mechanical Properties
Tensile Strength, Ultimate130 MPa 5 mm/min; ISO 527
Tensile Strength at Break130 MPa 0.2 in/min; ASTM D638
Elongation at Break3 % 0.2 in/min; ASTM D638
Elongation at Break3 % 5 mm/min; ISO 527
Tensile Modulus8.79 GPa ASTM D638
Tensile Modulus8.8 GPa 1 mm/min; ISO 527
Flexural Modulus7.8 GPa ASTM D790
Charpy Impact Unnotched5.5 J/cm² ISO 179
Charpy Impact, Notched, Low Temp0.85 J/cm² at -30°C; ISO 179
Charpy Impact, Unnotched Low Temp6 J/cm² at -30°C; ISO 179
Charpy Impact, Notched0.9 J/cm² ISO 179
Tensile Creep Modulus, 1 hour7500 MPa ISO 899
Tensile Creep Modulus, 1000 hours5800 MPa ISO 899
Izod Impact, Notched @ -40°C0.598 J/cm ASTM D256
Izod Impact, Notched0.598 J/m ASTM D256

Electrical Properties
Volume Resistivity1e+012 ohm-cm IEC 60093
Surface Resistance1e+012 ohm IEC 60093
Dielectric Constant4 100 Hz; IEC 60250
Dielectric Constant4 1 MHz; IEC 60250
Dielectric Strength43 kV/mm IEC 60243-1
Dissipation Factor0.002 100 Hz; IEC 60250
Dissipation Factor0.005 1 MHz; IEC 60250
Comparative Tracking Index600 V IEC 60112

Thermal Properties
CTE, linear 20°C20 µm/m-°C ASTM E831
CTE, linear 20°C30 µm/m-°C Parallel; ISO 11359
Melting Point168 °C ASTM D3418
Melting Point168 °C 10 K/min
Deflection Temperature at 0.46 MPa (66 psi)165 °C ASTM D648
Deflection Temperature at 0.46 MPa (66 psi)165 °C ISO 75
Deflection Temperature at 1.8 MPa (264 psi)160 °C ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)163 °C ISO 75
Vicat Softening Point160 °C (50 °C/h / 50N) - B/50; ISO 306
Flammability, UL94HB 1.5 mm
Flammability, UL94HB 3.0 mm

Descriptive Properties
ColorNatural 
Commercial Status (March 2007)Active America 
Impact ModifiedNo 
Primary Processing TechniqueInjection Molding 
Printer friendly version Printer friendly version


New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。