MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

BASF Ultraform W 2320 003 BK120 Q600 Acetal

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Acetal; Polymer; Thermoplastic

Material Notes:
Information provided by BASF Corporation.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesOriginal ValueComments
Density1.4 g/cc ISO 1183
Water Absorption0.8 % ISO 62
Moisture Absorption at Equilibrium0.2 % 23°C/50% R.H.; ISO 62
Linear Mold Shrinkage0.019 cm/cm MD; ASTM Test

Mechanical Properties
Tensile Strength, Yield63 MPa 50 mm/min; ISO 527
Elongation at Yield7.5 % 50 mm/min; ISO 527
Tensile Modulus2.7 GPa 1 mm/min; ISO 527
Flexural Modulus2.6 GPa ISO 178
Izod Impact, Notched (ISO)5.5 kJ/m² ISO 180
Charpy Impact, Notched0.55 J/cm² ISO 179

Thermal Properties
Melting Point167 °C ASTM D3418
Melting Point167 °C 10 K/min
Deflection Temperature at 1.8 MPa (264 psi)90 °C ISO 75

Descriptive Properties
ColorBK120 
Commercial Status (March 2007)Active America 
FDA21 CFR 177.2470 
Impact ModifiedNo 
Primary Processing TechniqueInjection Molding 
Printer friendly version Printer friendly version


New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。