MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

Arkema Group RILSAN® Fine Powders Polyamide 11

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 11; Polymer; Thermoplastic

Material Notes:
Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum products.
Typical Applications:

  • Shopping carts
  • Dishwasher baskets
  • Hand mixers
  • File rods
  • Wire shelves

Information provided by Arkema Group

Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate38 - 47 MPa 
Taber Abrasion, mg/1000 Cycles17 CS 17 wheel, 1 kg load

Electrical Properties
Volume Resistivity3.5e+014 ohm-cm 20°C and 65% RH at 500 V; ASTM D257
Surface Resistance2.4e+014 ohm 20°C and 65% RH at 500 V; ASTM D257
Dielectric Constant3.1 1 MHz
Dielectric Constant, Low Frequency3.9 100 Hz
Dielectric Strength30.5 kV/mm 0.4 mm thick

Thermal Properties
Heat of Fusion83.7 J/g 
CTE, linear 20°C150 µm/m-°C 

Descriptive Properties
Flammabilityself-extinguishing ASTM D 635 (measured at a thickness greater than 3mm to eliminate the influence of substrate)
Printer friendly version Printer friendly version


Free Trade Publications, Click Here!

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。