Arkema Rilsan® Powder ESY Black X 7260 Nylon 11, Coating Grade

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 11; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA11; Polyamide 11

Material Notes:
Powder ESY BLACK X 7260 - RILSAN POLYAMIDE 11 (PA11) POWDER

Melt mix black powder for coating of metallic parts by electrostatic spray, and post fused in an oven.

There is a wide range of colors.

The properties listed in the data base have been measured on a corresponding RILSAN PA11 Granule.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Density1.35 g/cc 
Water Absorption1.9 % 

Electrical Properties
Electrical Resistivity1e+014 ohm-cm 
Surface Resistance1e+014 ohm 
Dielectric Strength30 kV/mm 

Thermal Properties
Melting Point185 °C 10°C/min
Vicat Softening Point160 °C 50°C/hr; 50N
Flammability, UL94HB 1.6 mm
Flammability, UL94V-2 3.2 mm
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。