Arkema Rilsan® AESN TL Nylon 12, Flexible Tubing Grade (Dry)
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,EHL,22-010 Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized. High impact strength. Good chemical resistance. Very good ability to be processed at high speed. Example applications: For general use. ISO data provided by the manufacturer, Arkema.
| Physical Properties | Original Value | Comments |
|
| Density | 1.01 g/cc | |
| Water Absorption | 1.6 % | |
| Melt Flow | 2.5 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
| Tensile Strength, Yield | 48 MPa | 50 mm/min |
| Elongation at Break | Min 50 % | Nominal Strain; 50 mm/min |
| Elongation at Yield | 5 % | 50 mm/min |
| Tensile Modulus | 1.69 GPa | 1 mm/min |
Thermal Properties |
|
| Melting Point | 174 °C | 10°C/min |
| Flammability, UL94 | HB | 1.6 mm |
| Flammability, UL94 | V-2 | 3.2 mm |
|