Arkema Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Conditioned)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,EHLS,22-010,MD05 Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents. Low friction coefficient. No need of lubricant. Good impact strength. Easy to be processed. Example applications: Control cables tubing, parking brake control cable, cable for opening doors. ISO data provided by the manufacturer, Arkema.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.04 g/cc | |
Melt Flow | 1.6 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 46 MPa | 50 mm/min |
Elongation at Break | Min 50 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 7 % | 50 mm/min |
Tensile Modulus | 1.58 GPa | 1 mm/min |
Charpy Impact Unnotched | NB | |
Charpy Impact, Notched, Low Temp | 0.68 J/cm² | at -30°C |
Charpy Impact, Unnotched Low Temp | NB | |
Charpy Impact, Notched | 0.68 J/cm² | |
Electrical Properties |
|
Electrical Resistivity | 1e+014 ohm-cm | |
Surface Resistance | 1e+014 ohm | |
Thermal Properties |
|
CTE, linear 20°C | 90 µm/m-°C | Parallel to flow |
Melting Point | 174 °C | (Dry) |
Deflection Temperature at 0.46 MPa (66 psi) | 140 °C | |
Deflection Temperature at 1.8 MPa (264 psi) | 55 °C | |
Vicat Softening Point | 143 °C | 50°C/hr; 50N |
Flammability, UL94 | V-2 | 3.2 mm |
Flammability, UL94 | V-2 | 1.6 mm |
|
Printer friendly version |
|