Arkema Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Dry)
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MR,14-010 Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. mold-release agent. Good mechanical properties. Low friction coefficient. Easy filling of the mold due to its well adapted melt viscosity. Low shrinkage: include 1% on average for the design of the mold. Very good dimensional stability (low moisture absorption). High rate of production. UL classification: UL94 V2 (3,05mm) RTI(C) 65/65/65 Example applications: Stressed mechanical parts in all industrial field. ISO data provided by the manufacturer, Arkema.
Physical Properties | Original Value | Comments |
|
Density | 1.01 g/cc | |
Water Absorption | 1.6 % | |
Melt Flow | 69.4 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 42 MPa | 50 mm/min |
Elongation at Break | Min 50 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 8 % | 50 mm/min |
Tensile Modulus | 1.45 GPa | 1 mm/min |
Electrical Properties |
|
Dissipation Factor | 0.000306 | 1 MHz |
Dissipation Factor, Low Frequency | 0.000384 | 100 Hz |
Thermal Properties |
|
Melting Point | 174 °C | 10°C/min |
Flammability, UL94 | HB | 1.6 mm |
Flammability, UL94 | V-2 | 3.2 mm |
Oxygen Index | 21 % | |
|
Printer friendly version |
|