Arkema Rilsan® AMN G8 TLD Nylon 12, Graphite Filled (Dry)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLS,14-010,CD05

Rigid grade with graphite filler for injection molding. Available colors: steel gray. Light and heat stabilized. Mold-release agent.

Low friction coefficient. No need of lubricant. Good mechanical properties. Easy filling of the mold due to its well adapted viscosity. Low shrinkage: include 1% on average for the design of the mold. Very good dimensional stability (low moisture absorption). Higher rate of production.

Example applications: Moving mechanical parts.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Density1.02 g/cc 
Water Absorption1.6 % 
Melt Flow61.5 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield45 MPa 50 mm/min
Elongation at BreakMin 50 % Nominal Strain; 50 mm/min
Elongation at Yield10 % 50 mm/min
Tensile Modulus1.52 GPa 1 mm/min
Charpy Impact UnnotchedNB 
Charpy Impact, Notched, Low Temp0.4 J/cm² at -30°C
Charpy Impact, Unnotched Low TempNB 
Charpy Impact, Notched0.41 J/cm² 

Electrical Properties
Dissipation Factor0.000332 1 MHz
Dissipation Factor, Low Frequency0.00045 100 Hz

Thermal Properties
Melting Point174 °C 10°C/min
Flammability, UL94HB 3.1 mm
Flammability, UL94HB 1.6 mm
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。