Arkema Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Dry)
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12-P,MHLR,14-005 Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent. Good impact strength. Flexibility and dynamic properties. Easy filling of the mold due to its well adapted viscosity. Low shrinkage: include 1% on average for the design of the mold. Good dimensional stability (low moisture absorption). Example applications: Flexible parts with high impact strength and vibration resistance. ISO data provided by the manufacturer, Arkema.
Physical Properties | Original Value | Comments |
|
Density | 1.02 g/cc | |
Water Absorption | 1.4 % | |
Melt Flow | 42 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 31 MPa | 50 mm/min |
Elongation at Break | Min 50 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 20 % | 50 mm/min |
Tensile Modulus | 0.62 GPa | 1 mm/min |
Charpy Impact Unnotched | NB | |
Charpy Impact, Notched, Low Temp | 0.38 J/cm² | at -30°C |
Charpy Impact, Unnotched Low Temp | NB | |
Charpy Impact, Notched | 0.88 J/cm² | |
Electrical Properties |
|
Dissipation Factor | 0.000364 | 1 MHz |
Dissipation Factor, Low Frequency | 0.000742 | 100 Hz |
Thermal Properties |
|
Melting Point | 174 °C | 10°C/min |
Flammability, UL94 | HB | 3.1 mm |
Flammability, UL94 | HB | 1.6 mm |
|