MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

NetComposites

Arkema Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Dry)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLS,14-010,MD05

Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.

Low friction coefficient. Good impact strength. Easy filling of the mold due to its well adapted viscosity. Low shrinkage: include 1% on average for the design of the mold. Very good dimensional stability (low moisture absorption).

Example applications: Moving mechanical parts such as gear.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Density1.02 g/cc 
Water Absorption1.6 % 
Melt Flow50 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield46 MPa 50 mm/min
Elongation at BreakMin 50 % Nominal Strain; 50 mm/min
Elongation at Yield9 % 50 mm/min
Tensile Modulus1.5 GPa 1 mm/min

Electrical Properties
Dissipation Factor0.000326 1 MHz
Dissipation Factor, Low Frequency0.000298 100 Hz

Thermal Properties
Melting Point174 °C 10°C/min
Flammability, UL94HB 1.6 mm
Flammability, UL94V-2 3.2 mm
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。