Arkema Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Dry)
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MHLR,16-010 Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent. High impact strength. Easy filling of the mold due to its well adapted viscosity. Low shrinkage: include 1% on average for the design of the mold. Very good dimensional stability (low moisture absorption). Example applications: Parts for all technology with high impact strength requirements. ISO data provided by the manufacturer, Arkema.
Physical Properties | Original Value | Comments |
|
Density | 1.01 g/cc | |
Water Absorption | 1.6 % | |
Melt Flow | 5.3 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 41 MPa | 50 mm/min |
Elongation at Break | Min 50 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 9 % | 50 mm/min |
Tensile Modulus | 1.17 GPa | 1 mm/min |
Charpy Impact Unnotched | NB | |
Charpy Impact, Notched, Low Temp | 0.47 J/cm² | at -30°C |
Charpy Impact, Unnotched Low Temp | NB | |
Charpy Impact, Notched | 0.6 J/cm² | |
Thermal Properties |
|
Melting Point | 174 °C | 10°C/min |
Flammability, UL94 | HB | 1.6 mm |
Flammability, UL94 | V-2 | 3.2 mm |
|