Arkema Rilsan® ARVO 950 TLD Nylon 12, Rotomolding Grade (Conditioned)
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,RHLR,16-010 Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent. Easy to be processed in the same conditions as polyethylene. High thermal and chemical resistance. Outstanding mechanical properties. Low permeability to gas and hydrocarbon. Example applications: Oil tank, hydraulic fluid tank. ISO data provided by the manufacturer, Arkema.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.01 g/cc | |
Mechanical Properties |
|
Tensile Strength, Yield | 40 MPa | 50 mm/min |
Elongation at Break | Min 50 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 11 % | 50 mm/min |
Tensile Modulus | 1.08 GPa | 1 mm/min |
Charpy Impact Unnotched | NB | |
Charpy Impact, Notched, Low Temp | 0.59 J/cm² | at -30°C |
Charpy Impact, Unnotched Low Temp | NB | |
Charpy Impact, Notched | 0.67 J/cm² | |
Electrical Properties |
|
Electrical Resistivity | 1e+014 ohm-cm | |
Surface Resistance | 1e+014 ohm | |
Dielectric Strength | 30 kV/mm | |
Comparative Tracking Index | 600 V | |
Thermal Properties |
|
CTE, linear 20°C | 100 µm/m-°C | Parallel to flow |
Deflection Temperature at 0.46 MPa (66 psi) | 135 °C | |
Deflection Temperature at 1.8 MPa (264 psi) | 55 °C | |
Vicat Softening Point | 142 °C | 50°C/hr; 50N |
|