Arkema Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Dry)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,M,16-090,CF20 Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Antistatic properties. Example applications: Parts with high mechanical properties and dimensional precision. ISO data provided by the manufacturer, Arkema.
Physical Properties | Original Value | Comments |
|
Density | 1.1 g/cc | |
Melt Flow | 4.6 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Ultimate | 132 MPa | 5 mm/min |
Elongation at Break | 5 % | 5 mm/min |
Tensile Modulus | 12.6 GPa | 1 mm/min |
Charpy Impact Unnotched | 5.9 J/cm² | |
Charpy Impact, Notched, Low Temp | 1 J/cm² | at -30°C |
Charpy Impact, Unnotched Low Temp | 5.9 J/cm² | at -30°C |
Charpy Impact, Notched | 1.7 J/cm² | |
Thermal Properties |
|
Melting Point | 174 °C | 10°C/min |
Flammability, UL94 | HB | 3.1 mm |
Flammability, UL94 | HB | 1.6 mm |
|