Arkema Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Dry)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MHLR,16-020,GB30 Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent. Reinforced isotropic performances. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Low coefficient of linear expansion. Example applications: Mechanical parts with dimensional precision. ISO data provided by the manufacturer, Arkema.
Physical Properties | Original Value | Comments |
|
Density | 1.22 g/cc | |
Water Absorption | 1.2 % | |
Melt Flow | 70.8 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 42 MPa | 50 mm/min |
Elongation at Break | 24 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 5 % | 50 mm/min |
Tensile Modulus | 2.04 GPa | 1 mm/min |
Charpy Impact Unnotched | 3.8 J/cm² | |
Charpy Impact, Notched, Low Temp | 0.46 J/cm² | at -30°C |
Charpy Impact, Unnotched Low Temp | 4.45 J/cm² | at -30°C |
Charpy Impact, Notched | 0.5 J/cm² | |
Electrical Properties |
|
Dissipation Factor | 0.00029 | 1 MHz |
Dissipation Factor, Low Frequency | 0.00045 | 100 Hz |
Thermal Properties |
|
Melting Point | 174 °C | 10°C/min |
Flammability, UL94 | HB | 3.1 mm |
Flammability, UL94 | HB | 1.6 mm |
|