Arkema Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Conditioned)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MHLR,16-030,GF15 Rigid grade with glass fiber filler (15%) for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent. Rigidity combined with good impact strength. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability. Example applications: Mechanical fittings. ISO data provided by the manufacturer, Arkema.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Melt Flow | 12.9 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Ultimate | 72 MPa | 5 mm/min |
Elongation at Break | 8 % | 5 mm/min |
Tensile Modulus | 3.83 GPa | 1 mm/min |
Charpy Impact Unnotched | 6.4 J/cm² | |
Charpy Impact, Notched, Low Temp | 0.72 J/cm² | at -30°C |
Charpy Impact, Unnotched Low Temp | 6.87 J/cm² | at -30°C |
Charpy Impact, Notched | 1.15 J/cm² | |
Thermal Properties |
|
Vicat Softening Point | 151 °C | 50°C/hr; 50N |
|