Arkema Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Dry)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MHLR,16-050,GF23 Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-release agent. Rigidity. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability. Example applications: Rigid mechanical parts. ISO data provided by the manufacturer, Arkema.
Physical Properties | Original Value | Comments |
|
Melt Flow | 3.2 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Ultimate | 85 MPa | 5 mm/min |
Elongation at Break | 6 % | 5 mm/min |
Tensile Modulus | 5.48 GPa | 1 mm/min |
Electrical Properties |
|
Dissipation Factor | 0.000357 | 1 MHz |
Dissipation Factor, Low Frequency | 0.000522 | 100 Hz |
|