Arkema Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Dry)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MHLR,16-060,GF30 Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent. High rigidity. High compressive strength. Good thermal properties. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability. UL classification: UL94 HB (3,05mm) RTI(C) 110/105/110 Example applications: Quick connectors. ISO data provided by the manufacturer, Arkema.
Physical Properties | Original Value | Comments |
|
Density | 1.24 g/cc | |
Water Absorption | 1.2 % | |
Melt Flow | 4.8 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Ultimate | 112 MPa | 5 mm/min |
Elongation at Break | 5 % | 5 mm/min |
Tensile Modulus | 8 GPa | 1 mm/min |
Electrical Properties |
|
Dielectric Strength | 35.5 kV/mm | |
Dissipation Factor | 0.000345 | 1 MHz |
Dissipation Factor, Low Frequency | 0.0004 | 100 Hz |
Comparative Tracking Index | 600 V | |
Thermal Properties |
|
Melting Point | 174 °C | 10°C/min |
Flammability, UL94 | HB | 3.1 mm |
Flammability, UL94 | HB | 1.6 mm |
|
Printer friendly version |
|