Arkema Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Dry)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05) Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stabilizing agent. Mold-release agent. High rigidity. Low friction coefficient. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability. Example applications: Mechanical parts with friction such as gear and bearing. ISO data provided by the manufacturer, Arkema.
Physical Properties | Original Value | Comments |
|
Density | 1.39 g/cc | |
Water Absorption | 1 % | |
Melt Flow | 2.3 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Ultimate | 138 MPa | 5 mm/min |
Elongation at Break | 4 % | 5 mm/min |
Tensile Modulus | 13.3 GPa | 1 mm/min |
Charpy Impact Unnotched | 6.87 J/cm² | |
Charpy Impact, Notched, Low Temp | 1.06 J/cm² | at -30°C |
Charpy Impact, Unnotched Low Temp | 6.87 J/cm² | at -30°C |
Charpy Impact, Notched | 1.26 J/cm² | |
Thermal Properties |
|
Melting Point | 174 °C | 10°C/min |
Flammability, UL94 | HB | 3.1 mm |
Flammability, UL94 | HB | 1.6 mm |
|