Arkema Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05) Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stabilizing agent. Mold-release agent. High rigidity. Low friction coefficient. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability. Example applications: Mechanical parts with friction such as gear and bearing. ISO data provided by the manufacturer, Arkema.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.39 g/cc | |
Melt Flow | 2.3 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Ultimate | 135 MPa | 5 mm/min |
Elongation at Break | 4 % | 5 mm/min |
Tensile Modulus | 12.4 GPa | 1 mm/min |
Charpy Impact Unnotched | 7.12 J/cm² | |
Charpy Impact, Notched, Low Temp | 1.06 J/cm² | at -30°C |
Charpy Impact, Unnotched Low Temp | 7.25 J/cm² | at -30°C |
Charpy Impact, Notched | 1.27 J/cm² | |
Electrical Properties |
|
Electrical Resistivity | 1e+012 ohm-cm | |
Surface Resistance | 1e+011 ohm | |
Dielectric Strength | 20 kV/mm | |
Comparative Tracking Index | 275 V | |
Thermal Properties |
|
CTE, linear 20°C | 30 µm/m-°C | Parallel to flow |
Melting Point | 174 °C | (Dry) |
Deflection Temperature at 0.46 MPa (66 psi) | 173 °C | |
Deflection Temperature at 1.8 MPa (264 psi) | 170 °C | |
Vicat Softening Point | 165 °C | 50°C/hr; 50N |
Flammability, UL94 | HB | 3.1 mm |
Flammability, UL94 | HB | 1.6 mm |
|