MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

Arkema Rilsan® MA 4420 Nylon 12, Flexible Tubing Grade (Dry)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA11; Polyamide 11

Material Notes:
Designation ISO 1874-PA12-HI,EHL,22-003

Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized.

Flexibility. High burst pressure and impact strength. Fit for use in a wide range of temperature. Very good chemical resistance.

Example applications: Tubes for air brake system in trucks approved by ISO 7628, DIN 73378 (PA12-PHLY), NFR 12632, SAEJ 844.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Water Absorption1.2 % 
Moisture Absorption at Equilibrium0.55 % Humidity Absorption
Melt Flow4.8 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield33 MPa 50 mm/min
Elongation at BreakMin 50 % Nominal Strain; 50 mm/min
Elongation at Yield19 % 50 mm/min
Tensile Modulus0.72 GPa 1 mm/min
Charpy Impact UnnotchedNB 
Charpy Impact, Notched, Low Temp0.43 J/cm² at -30°C
Charpy Impact, Unnotched Low TempNB 
Charpy Impact, Notched1.6 J/cm² 

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)42 °C 
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。