Arkema Rilsan® MA 4420 Nylon 12, Flexible Tubing Grade (Conditioned)
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA11; Polyamide 11
Material Notes: Designation ISO 1874-PA12-HI,EHL,22-003 Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized. Flexibility. High burst pressure and impact strength. Fit for use in a wide range of temperature. Very good chemical resistance. Example applications: Tubes for air brake system in trucks approved by ISO 7628, DIN 73378 (PA12-PHLY), NFR 12632, SAEJ 844. ISO data provided by the manufacturer, Arkema.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Melt Flow | 4.8 g/10 min | 235°C/2.16 kg load |
Mechanical Properties |
|
Tensile Strength, Yield | 31 MPa | 50 mm/min |
Elongation at Break | Min 50 % | Nominal Strain; 50 mm/min |
Elongation at Yield | 21 % | 50 mm/min |
Tensile Modulus | 0.64 GPa | 1 mm/min |
Charpy Impact Unnotched | NB | |
Charpy Impact, Notched, Low Temp | 0.54 J/cm² | at -30°C |
Charpy Impact, Unnotched Low Temp | NB | |
Charpy Impact, Notched | 2.79 J/cm² | |
|