LANXESS Pocan® KU 2-7426 PET
Subcategory: Filled/Reinforced Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polymer; Thermoplastic
Close Analogs: LANXESS was spun-off from Bayer in early 2005.
Material Notes: Key Features: Suitable processing methods: Information provided by Bayer Polymers.
| Physical Properties | Original Value | Comments |
|
| Density | 1.55 g/cc | |
| Water Absorption | 0.3 % | |
| Moisture Absorption at Equilibrium | 0.1 % | 23°C/50% R.H. |
| Melt Flow | 35 g/10 min | (cm³/10 min.) 260°C/2.16 kg |
Mechanical Properties |
|
| Tensile Strength, Ultimate | 130 MPa | |
| Elongation at Break | 2 % | |
| Tensile Modulus | 9.6 GPa | |
Thermal Properties |
|
| Melting Point | 250 °C | 10°C/min |
| Vicat Softening Point | 235 °C | 50°C/h 50N |
| Flammability, UL94 | V-2 | 1.6 mm |
Processing Properties |
|
| Melt Temperature | 270 °C | Injection Molding |
| Mold Temperature | 130 °C | Injection Molding |
| Injection Velocity | 200 mm/sec | |
|