Bayer MaterialScience Texin® 270 Urethane Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU
Material Notes: Key Features: Suitable processing methods: Information provided by Bayer Polymers.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.24 g/cc | |
Mechanical Properties |
|
Tensile Strength, Yield | 28 MPa | Stress at 50% Strain |
Elongation at Break | Min 50 % | |
Electrical Properties |
|
Volume Resistivity | 5e+012 ohm-cm | |
Surface Resistance | 9e+014 ohm | |
Dielectric Constant | 3.9 | 1 MHz |
Dielectric Constant | 4.6 | 100 Hz |
Dielectric Strength | 23.7 kV/mm | |
Dissipation Factor | 0.029 | 1 MHz |
Dissipation Factor | 0.031 | 100 Hz |
Thermal Properties |
|
CTE, linear 20°C | 140 µm/m-°C | Parallel |
Deflection Temperature at 0.46 MPa (66 psi) | 46 °C | |
Vicat Softening Point | 158 °C | 50°C/h 50N |
Glass Temperature | 0 °C | 10°C/min |
Processing Properties |
|
Melt Temperature | 230 °C | Injection Molding |
Mold Temperature | 35 °C | Injection Molding |
Injection Pressure | 45 MPa | |
|
Printer friendly version |
|