MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

Bayer MaterialScience Texin® 285 Urethane Thermoplastic Elastomer

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU

Material Notes:
Key Features:

  • Unfilled

Suitable processing methods:

  • Injection molding
  • Film extrusion
  • Profile extrusion
  • Sheet extrusion
  • Coating
  • Blow molding

Information provided by Bayer Polymers.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesOriginal ValueComments
Density1.2 g/cc 

Mechanical Properties
Tensile Strength, Yield5 MPa Stress at 50% Strain
Elongation at BreakMin 50 % 

Electrical Properties
Volume Resistivity8e+009 ohm-cm 
Surface Resistance5e+011 ohm 
Dielectric Constant5.6 1 MHz
Dielectric Constant6.5 100 Hz
Dielectric Strength17.5 kV/mm 
Dissipation Factor0.025 100 Hz
Dissipation Factor0.06 1 MHz

Thermal Properties
CTE, linear 20°C150 µm/m-°C Parallel
Vicat Softening Point91 °C 50°C/h 50N
Glass Temperature-42 °C 10°C/min
Flammability, UL94HB 1.5 mm UL Recognized
Flammability, UL94V-2 3 mm UL Recognized

Processing Properties
Melt Temperature200 °C Injection Molding
Mold Temperature30 °C Injection Molding
Injection Pressure45 MPa 
Printer friendly version Printer friendly version


New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。