Bayer MaterialScience Texin® 970U Urethane Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU
Material Notes: Key Features:- Unfilled
- U.V. stabilized or stable to weather
Suitable processing methods: - Injection molding
- Profile extrusion
- Sheet extrusion
Information provided by Bayer Polymers.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.18 g/cc | |
Thermal Properties |
|
| CTE, linear 20°C | 90 µm/m-°C | Parallel |
| Deflection Temperature at 0.46 MPa (66 psi) | 68 °C | |
| Deflection Temperature at 1.8 MPa (264 psi) | 45 °C | |
| Vicat Softening Point | 140 °C | 50°C/h 50N |
| Glass Temperature | 0 °C | 10°C/min |
Processing Properties |
|
| Melt Temperature | 230 °C | Injection Molding |
| Mold Temperature | 35 °C | Injection Molding |
| Injection Pressure | 45 MPa | |
|