Bayer MaterialScience Texin® 985U Urethane Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU
Material Notes: Key Features:- Unfilled
- U.V. stabilized or stable to weather
Suitable processing methods: - Injection molding
- Film extrusion
- Profile extrusion
- Sheet extrusion
- Blow molding
Information provided by Bayer Polymers.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.12 g/cc | |
Mechanical Properties |
|
Tensile Strength, Yield | 5 MPa | Stress at 50% Strain |
Elongation at Break | Min 50 % | |
Thermal Properties |
|
Vicat Softening Point | 80 °C | 50°C/h 50N |
Glass Temperature | -46 °C | 10°C/min |
Processing Properties |
|
Melt Temperature | 195 °C | Injection Molding |
Mold Temperature | 35 °C | Injection Molding |
Injection Pressure | 45 MPa | |
|