Bayer MaterialScience Texin® 4215 Urethane Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU
Material Notes: Key Features: Suitable processing methods: - Injection molding
- Film extrusion
- Profile extrusion
- Sheet extrusion
Information provided by Bayer Polymers.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.21 g/cc | |
Mechanical Properties |
|
Tensile Strength, Yield | 21 MPa | Stress at 50% Strain |
Elongation at Break | Min 50 % | |
Thermal Properties |
|
CTE, linear 20°C | 115 µm/m-°C | Parallel |
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | |
Deflection Temperature at 1.8 MPa (264 psi) | 74 °C | |
Vicat Softening Point | 140 °C | 50°C/h 50N |
Glass Temperature | -35 °C | 10°C/min |
Flammability, UL94 | HB | 1.5 mm UL Recognized |
Processing Properties |
|
Melt Temperature | 230 °C | Injection Molding |
Mold Temperature | 35 °C | Injection Molding |
Injection Pressure | 45 MPa | |
|