DSM Engineering Plastics Stanyl® 46HF5041LW (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow, Low Warpage (North America)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic
Key Words: Polyamide 46
Material Notes: Information provided by DSM Engineering Plastics.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.87 g/cc | ISO 1183 |
| Moisture Absorption at Equilibrium | 1.1 % | 50% RH / 23°C; Similar to ISO 62 |
Mechanical Properties |
|
| Tensile Strength at Break | 150 MPa | ISO 527-1/-2 |
| Elongation at Break | 1.3 % | ISO 527-1/-2 |
| Tensile Modulus | 16 GPa | ISO 527-1/-2 |
| Charpy Impact Unnotched | 2.5 J/cm² | ISO 179/1eU |
| Charpy Impact, Notched | 0.8 J/cm² | ISO 179/1eU |
Thermal Properties |
|
| CTE, linear 20°C | 20 µm/m-°C | parallel to flow; ISO 11359-1/-2 |
| CTE, linear 20°C Transverse to Flow | 80 µm/m-°C | ISO 11359-1/-2 |
| Melting Point | 295 °C | ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 270 °C | ISO 75-1/-2 |
| UL RTI, Electrical | 140 °C | 1.5 mm; UL746B |
| Flammability, UL94 | V-0 | 0.4 mm |
|