DSM Engineering Plastics Stanyl® 46HF5050 (DAM) Nylon 46 50% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic
Key Words: Polyamide 46
Material Notes: Information provided by DSM Engineering Plastics.
Physical Properties | Original Value | Comments |
|
Density | 1.87 g/cc | ISO 1183 |
Moisture Absorption at Equilibrium | 1.1 % | 50% RH / 23°C; Similar to ISO 62 |
Mechanical Properties |
|
Tensile Strength at Break | 200 MPa | ISO 527-1/-2 |
Elongation at Break | 1.5 % | ISO 527-1/-2 |
Tensile Modulus | 18 GPa | ISO 527-1/-2 |
Thermal Properties |
|
CTE, linear 20°C | 20 µm/m-°C | parallel to flow; ISO 11359-1/-2 |
CTE, linear 20°C Transverse to Flow | 80 µm/m-°C | ISO 11359-1/-2 |
Melting Point | 295 °C | ISO 11357-1/-3 |
Deflection Temperature at 1.8 MPa (264 psi) | 290 °C | ISO 75-1/-2 |
UL RTI, Electrical | 140 °C | 1.5 mm; UL746B |
Flammability, UL94 | V-0 | 0.4 mm |
|
Printer friendly version |
|