DSM Engineering Plastics Stanyl® TE250F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic
Key Words: Polyamide 46
Material Notes: Information provided by DSM Engineering Plastics.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.68 g/cc | (DAM); ISO 1183 |
Mechanical Properties |
|
| Tensile Strength at Break | 125 MPa | ISO 527-1/-2 |
| Elongation at Break | 3.5 % | ISO 527-1/-2 |
| Tensile Modulus | 8 GPa | ISO 527-1/-2 |
| Charpy Impact Unnotched | 6 J/cm² | ISO 179/1eU |
| Charpy Impact, Notched, Low Temp | 0.9 J/cm² | at -30°C; ISO 179/1eU |
| Charpy Impact, Unnotched Low Temp | 5 J/cm² | at -30°C; ISO 179/1eU |
| Charpy Impact, Notched | 1.1 J/cm² | ISO 179/1eU |
Electrical Properties |
|
| Volume Resistivity | 1e+008 ohm-cm | IEC 60093 |
| Dielectric Strength | 20 kV/mm | IEC 60243-1 |
| Comparative Tracking Index | 325 V | IEC 60112 |
Thermal Properties |
|
| Melting Point | 295 °C | (DAM); ISO 11357-1/-3 |
|
Printer friendly version |

|