DSM Engineering Plastics Stanyl® TW200F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic

Key Words: Polyamide 46

Material Notes:
Information provided by DSM Engineering Plastics.

Physical PropertiesOriginal ValueComments
Density1.41 g/cc ISO 1183
Moisture Absorption at Equilibrium2.6 % 50% RH / 23°C; Similar to ISO 62

Mechanical Properties
Tensile Strength at Break210 MPa ISO 527-1/-2
Elongation at Break4 % ISO 527-1/-2
Tensile Modulus10 GPa ISO 527-1/-2
Charpy Impact Unnotched8 J/cm² ISO 179/1eU
Charpy Impact, Notched, Low Temp1 J/cm² at -30°C; ISO 179/1eU
Charpy Impact, Unnotched Low Temp7 J/cm² at -30°C; ISO 179/1eU
Charpy Impact, Notched1.2 J/cm² ISO 179/1eU

Electrical Properties
Volume Resistivity1e+012 ohm-cm IEC 60093
Dielectric Strength30 kV/mm IEC 60243-1
Comparative Tracking Index300 V IEC 60112

Thermal Properties
CTE, linear 20°C20 µm/m-°C parallel to flow; ISO 11359-1/-2
CTE, linear 20°C Transverse to Flow80 µm/m-°C ISO 11359-1/-2
Melting Point295 °C ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi)290 °C ISO 75-1/-2
Printer friendly version Printer friendly version


Free Trade Publications, Click Here!

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。