DSM Engineering Plastics Stanyl® TW200F8 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic
Key Words: Polyamide 46
Material Notes: Information provided by DSM Engineering Plastics.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.51 g/cc | (DAM); ISO 1183 |
Mechanical Properties |
|
Tensile Strength at Break | 140 MPa | ISO 527-1/-2 |
Elongation at Break | 6 % | ISO 527-1/-2 |
Tensile Modulus | 8 GPa | ISO 527-1/-2 |
Charpy Impact Unnotched | 9.5 J/cm² | ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 1.2 J/cm² | at -30°C; ISO 179/1eU |
Charpy Impact, Unnotched Low Temp | 7.5 J/cm² | at -30°C; ISO 179/1eU |
Charpy Impact, Notched | 2.2 J/cm² | ISO 179/1eU |
Electrical Properties |
|
Volume Resistivity | 1e+008 ohm-cm | IEC 60093 |
Dielectric Strength | 20 kV/mm | IEC 60243-1 |
Comparative Tracking Index | 300 V | IEC 60112 |
Thermal Properties |
|
Melting Point | 295 °C | (DAM); ISO 11357-1/-3 |
|