DSM Engineering Plastics Stanyl® TW241F12 (COND) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic
Key Words: Polyamide 46
Material Notes: Information provided by DSM Engineering Plastics.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.76 g/cc | (DAM); ISO 1183 |
Mechanical Properties |
|
Tensile Strength at Break | 170 MPa | ISO 527-1/-2 |
Elongation at Break | 3 % | ISO 527-1/-2 |
Tensile Modulus | 12 GPa | ISO 527-1/-2 |
Charpy Impact Unnotched | 10 J/cm² | ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 1.9 J/cm² | at -30°C; ISO 179/1eU |
Charpy Impact, Unnotched Low Temp | 8 J/cm² | at -30°C; ISO 179/1eU |
Charpy Impact, Notched | 2 J/cm² | ISO 179/1eU |
Thermal Properties |
|
Melting Point | 295 °C | (DAM); ISO 11357-1/-3 |
|