DSM Engineering Plastics Stanyl® TW275F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Molydisulfide Lubricated (North America)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic
Key Words: Polyamide 46
Material Notes: Information provided by DSM Engineering Plastics.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.43 g/cc | (DAM); ISO 1183 |
Mechanical Properties |
|
| Tensile Strength at Break | 115 MPa | ISO 527-1/-2 |
| Elongation at Break | 7 % | ISO 527-1/-2 |
| Tensile Modulus | 6 GPa | ISO 527-1/-2 |
| Flexural Modulus | 6 GPa | ISO 178 |
| Izod Impact, Notched (ISO) | 15 kJ/m² | ISO 180/1A |
| Izod Impact, Notched, Low Temp (ISO) | 8 kJ/m² | at -40°C; ISO 180/1A |
Thermal Properties |
|
| Melting Point | 295 °C | (DAM); ISO 11357-1/-3 |
|