DSM Engineering Plastics Stanyl® TW363 (DAM) Nylon 46 Heat Stabilized, Impact Modified (North America)
Subcategory: Nylon; Nylon 46; Polymer; Thermoplastic
Key Words: Polyamide 46
Material Notes: Information provided by DSM Engineering Plastics.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.1 g/cc | ISO 1183 |
Moisture Absorption at Equilibrium | 3 % | 50% RH / 23°C; Similar to ISO 62 |
Mechanical Properties |
|
Tensile Strength, Yield | 60 MPa | ISO 527-1/-2 |
Elongation at Yield | Min 50 % | Nominal Strain at Yield; ISO 527-1/-2 |
Tensile Modulus | 1.85 GPa | ISO 527-1/-2 |
Charpy Impact Unnotched | NB | ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 2.6 J/cm² | at -30°C; ISO 179/1eU |
Charpy Impact, Unnotched Low Temp | NB | at -30°C; ISO 179/1eU |
Charpy Impact, Notched | 7.5 J/cm² | ISO 179/1eU |
Electrical Properties |
|
Volume Resistivity | 1e+013 ohm-cm | IEC 60093 |
Dielectric Strength | 25 kV/mm | IEC 60243-1 |
Comparative Tracking Index | 475 V | IEC 60112 |
Thermal Properties |
|
CTE, linear 20°C | 160 µm/m-°C | parallel to flow; ISO 11359-1/-2 |
CTE, linear 20°C Transverse to Flow | 180 µm/m-°C | ISO 11359-1/-2 |
Melting Point | 295 °C | ISO 11357-1/-3 |
Deflection Temperature at 1.8 MPa (264 psi) | 90 °C | ISO 75-1/-2 |
|