MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

DSM Stanyl® TS256F8 Nylon 46-40% Glass Reinforced (Asian Grade) (Dry)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic

Material Notes:
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:

  • Highest mechanical properties at high temperatures
  • Excellent resistance to wear and low friction
  • Outstanding flow for easy processing and exceptional design freedom
  • Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties

Key Applications:

  • Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensioners
  • E&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliances

    Information provided by DSM.

    No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

    Physical PropertiesOriginal ValueComments
    Density1.65 g/cc ISO 1183
    Moisture Absorption at Equilibrium1.2 % Similar to ISO 62

    Mechanical Properties
    Tensile Strength at Break180 MPa ISO 527-1/-2
    Elongation at Break2 % ISO 527-1/-2
    Tensile Modulus14 GPa ISO 527-1/-2
    Charpy Impact, Notched, Low Temp0.8 J/cm² At -30°C; ISO 179/1eA
    Charpy Impact, Notched0.8 J/cm² At 23°C; ISO 179/1eA

    Thermal Properties
    CTE, linear 20°C20 µm/m-°C ISO 11359-1/-2
    CTE, linear 20°C Transverse to Flow70 µm/m-°C ISO 11359-1/-2
    Melting Point295 °C 10°C/min; ISO 11357-1/-3
    Deflection Temperature at 1.8 MPa (264 psi)290 °C ISO 75-1/-2
    Flammability, UL94V-0 0.75 mm; IEC 60695-11-10
    Printer friendly version Printer friendly version


    New MatWeb Services

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
  • 请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。