DSM Stanyl® TW241F3 Nylon 46-15% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic
Material Notes: Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:- Highest mechanical properties at high temperatures
- Excellent resistance to wear and low friction
- Outstanding flow for easy processing and exceptional design freedom
- Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties
Key Applications: Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensionersE&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliancesInformation provided by DSM.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.29 g/cc | ISO 1183 |
Mechanical Properties |
|
Tensile Strength at Break | 140 MPa | ISO 527-1/-2 |
Elongation at Break | 4 % | ISO 527-1/-2 |
Tensile Modulus | 6.1 GPa | ISO 527-1/-2 |
Thermal Properties |
|
CTE, linear 20°C | 30 µm/m-°C | ISO 11359-1/-2 |
CTE, linear 20°C Transverse to Flow | 90 µm/m-°C | ISO 11359-1/-2 |
Melting Point | 295 °C | 10°C/min; ISO 11357-1/-3 |
Deflection Temperature at 1.8 MPa (264 psi) | 275 °C | ISO 75-1/-2 |
|