DSM Stanyl® TW241F8 Nylon 46-40% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic
Material Notes: Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:- Highest mechanical properties at high temperatures
- Excellent resistance to wear and low friction
- Outstanding flow for easy processing and exceptional design freedom
- Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties
Key Applications: Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensionersE&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliancesInformation provided by DSM.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.51 g/cc | ISO 1183 |
Linear Mold Shrinkage | 0.005 cm/cm | Parallel; ISO 294-4 |
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | Normal; ISO 194-4 |
Mechanical Properties |
|
Tensile Strength at Break | 230 MPa | ISO 527-1/-2 |
Elongation at Break | 3 % | ISO 527-1/-2 |
Tensile Modulus | 13 GPa | ISO 527-1/-2 |
Charpy Impact Unnotched | 8.5 J/cm² | At 23°C; ISO 179/1eA |
Charpy Impact, Notched, Low Temp | 1.2 J/cm² | At -30°C; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | 7.5 J/cm² | At -30°C; ISO 179/1eA |
Charpy Impact, Notched | 1.4 J/cm² | At 23°C; ISO 179/1eA |
Thermal Properties |
|
CTE, linear 20°C | 20 µm/m-°C | ISO 11359-1/-2 |
CTE, linear 20°C Transverse to Flow | 80 µm/m-°C | ISO 11359-1/-2 |
Melting Point | 295 °C | 10°C/min; ISO 11357-1/-3 |
Deflection Temperature at 1.8 MPa (264 psi) | 290 °C | ISO 75-1/-2 |
Flammability, UL94 | HB | 0.75 mm; IEC 60695-11-10 |
|