DuPont Zytel® 159 NC010 Nylon 612

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)Material suppliers Material suppliers
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 612; Polymer; Thermoplastic

Material Notes:
Zytel® 159 NC010 is a high viscosity polyamide 612 resin that is suitable for extrusion applications, such as monofilaments and tubing.

Click here to view available vendors for this material.

DuPont Performance Polymers can be your partner to help you carry a project from concept to commercialization. Our products bridge the gap between often costly high-performance specialty polymers and metals.

Physical PropertiesMetricEnglishComments
Density1.06 g/cc0.0383 lb/in³ DAM; ISO 1183
Water Absorption0.45 %0.45 % Immersion 24h; 23°C; DAM; ISO 62, Similar to

Mechanical Properties
Tensile Strength, Yield62 MPa8990 psi DAM; ISO 527
Elongation at Break35 %35 % DAM; Nominal; ISO 527
Elongation at Yield4.5 %4.5 % ISO 527
Tensile Modulus2.4 GPa348 ksi DAM; ISO 527
Flexural Modulus2.15 GPa312 ksi DAM; ISO 178
Charpy Impact, Notched0.5 J/cm²2.38 ft-lb/in² DAM; ISO 179/1eA

Thermal Properties
Melting Point216 °C421 °F 10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi)62 °C144 °F DAM; ISO 75-1/-2

Processing Properties
Melt Temperature230 - 290 °C446 - 554 °F 
Melt Temperature250 °C482 °F Optimum
Mold Temperature50 - 90 °C122 - 194 °F 
Mold Temperature70 °C158 °F Optimum
Drying Temperature80 °C176 °F 
Dry Time2 - 4 hour2 - 4 hour Dehumidified Dryer
Moisture ContentMax 0.05 %Max 0.05 % 

Descriptive Properties
DryingRecommended If moisture content of resin exceeds recommended level
DuPont Product CategoryExtrusion Resins 
DuPont Product CategoryUnreinforced Resins 
FormPellets 
RegionAmericas 
RegionAsia/Pacific 
RegionEurope 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ASM International

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。